Polymer Property : Pour Point = -4.00 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Pour Point -4.00 °C
24.8 °F
ChevronTexaco Pinnacle® 680
Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o..
Pour Point -4.00 °C
24.8 °F
ChevronTexaco Pinnacle® 460
Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o..
Pour Point -4.00 °C
24.8 °F
ASTM D97
ChevronTexaco Bright-Cut® AM Metal Working Fluid
FeaturesChevron Bright-Cut Metalworking Fluids are a complete line of chlorine-free cutting oils that offer benefits not found in conventional cutting oils.The unique synthetic antiweld components ..