Polymer Property : Pour Point = -4.00 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Pour Point -20.0 °C
-4.00 °F
Base Oil; ASTM D97
Nye Lubricants 171B (SO) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -20.0 °C
-4.00 °F
Base Oil; ASTM D97
Nye Lubricants 176L (SO) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -20.0 °C
-4.00 °F
Base Oil; ASTM D97
Nye Lubricants 327A (SO) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -20.0 °C
-4.00 °F
Base Oil; ASTM D97
Nye Lubricants 573H-40 (NT) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -20.0 °C
-4.00 °F
Base Oil; ASTM D97
Nye Lubricants 731 (IG) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -20.0 °C
-4.00 °F
Base Oil; ASTM D97
Nye Lubricants NC-140 Grease
Information provided by Nye Lubricants.
Pour Point -20.0 °C
-4.00 °F
Base Oil; ASTM D97
Nye Lubricants PG-1S Grease
Information provided by Nye Lubricants.
Pour Point -20.0 °C
-4.00 °F
Base Oil; ASTM D97
Nye Lubricants PG-2S Grease
Information provided by Nye Lubricants.
Pour Point -20.0 °C
-4.00 °F
Base Oil; ASTM D97
Nye Lubricants PG-3S Grease
Information provided by Nye Lubricants.
Pour Point -20.0 °C
-4.00 °F
Base Oil; ASTM D97
Nye Lubricants PG-4S Grease
Information provided by Nye Lubricants.
Pour Point -20.0 °C
-4.00 °F
Base Oil; ASTM D97
Nye Lubricants PG-8S Grease
Information provided by Nye Lubricants.
Pour Point -20.0 °C
-4.00 °F
Base Oil; ASTM D97
Nye Lubricants UniFlor 8620 (496A) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -20.0 °C
-4.00 °F
Base Oil; ASTM D97
Nye Lubricants UniFlor 8622 (851) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -20.0 °C
-4.00 °F
Base Oil; ASTM D97
Nye Lubricants UniFlor 8622R (851RP) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -20.0 °C
-4.00 °F
Base Oil; ASTM D97
Nye Lubricants UniFlor 8623 (717C) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -20.0 °C
-4.00 °F
Base Oil; ASTM D97
Nye Lubricants UniFlor 8623G (UF) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -20.0 °C
-4.00 °F
PolyOne Synplast™ 901P-N Di (Nonyl, Decyl, Undecyl) Phthalate
Linear phthalate esterInformation provided by PolyOne
Pour Point -20.0 °C
-4.00 °F
Solvay RHODAFAC® ARB/70 Surfactant
Description: High concentration specific biological activator for Glyphosate based herbicide SL formulation.Identification: PHOSPHATE ESTERAvailable in: Asia Pacific, Europe, Latin America and North..
Pour Point <= -20.0 °C
<= -4.00 °F
RP-0461
Solvay RHODAFAC® LO-11/ALA Surfactant
Description: Phosphate ester designed for use in diesel and crude oils, where it will react with specific organometalic complexors to form very high viscosity crosslinked oil gels.Chemical Name: ALK..
Pour Point -20.0 °C
-4.00 °F
ExxonMobil Mobilmet S-122
Mobilmet S-122 is a water-soluble, general-purpose cutting oil designed for moderate-duty cutting and metalworking operations. Mobilmet S-122 fluid is formulated with select base oils and fortifie..
Pour Point -20.0 °C
-4.00 °F
ExxonMobil Unirex PF 500
Formulated with perfluoropolyether that has been thickened with a non-organic polytetrafluoroethylene, UNIREX PF 500 is a long-life, severe-service grease for bearings, valves, seals and other appli..
Pour Point -20.0 °C
-4.00 °F
ASTM D97
ELM® SoyLube® All Purpose Lubricant and Penetrating Oil
Description: SoyLube All Purpose Lubricant and Penetrating Oil is a high performance, biodegradable penetrant and lubricating oil for general purpose use. Formulated with the best optimized USA-gro..
Pour Point -20.0 °C
-4.00 °F
ExxonMobil Mobilmet S-122
Mobilmet S-122 is a water-soluble, general-purpose cutting oil designed for moderate-duty cutting and metalworking operations. Mobilmet S-122 fluid is formulated with select base oils and fortifie..
Pour Point -20.0 °C
-4.00 °F
ExxonMobil Unirex PF 500
Formulated with perfluoropolyether that has been thickened with a non-organic polytetrafluoroethylene, UNIREX PF 500 is a long-life, severe-service grease for bearings, valves, seals and other appli..
Pour Point -20.0 °C
-4.00 °F
ASTM D-97
ConocoPhillips ANDEROL® AA-30 White Mineral Food Grade Oil, ISO Grade 68/100, SAE Grade 30
Description: ANDEROL PQ AA Series Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Oils are ..
Pour Point -20.0 °C
-4.00 °F
ASTM D-97
ConocoPhillips ANDEROL® AA-40 White Mineral Food Grade Oil, ISO Grade 150, SAE Grade 40
Description: ANDEROL PQ AA Series Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Oils are ..
Pour Point -20.0 °C
-4.00 °F
ChevronTexaco Cepheus® 220
Texaco Cepheus oil deliver value throughThe ability to retain lubrication properties in the presence of water.Good rust protection from a carefully designed additive package.The ease with which they..
Pour Point -20.0 °C
-4.00 °F
PolyOne Synplast™ 901P-E Di (Nonyl, Decyl, Undecyl) Phthalate
Linear phthalate esterNote: Contains 0.1 - 0.15 wt% 1,1,3-Tris (2-methyl-4-hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne