Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -52.0 °C | -61.6 °F | Base Oil; ASTM D97 |
Nye Lubricants 300 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -52.0 °C | -61.6 °F | |
ChevronTexaco Pinnacle® 68 Texaco Pinnacle oils deliver value through:Long lubricant life in high temperature operations — The synthetic hydrocarbon base oils and proprietary additive package used in these products provide o.. |
|||
Pour Point | <= -52.0 °C | <= -61.6 °F | ASTM D97 |
ChevronTexaco Supreme SAE 5W-30 Synthetic Motor Oil FeaturesChevron Supreme 100% Synthetic Motor Oils are designed for those drivers who demand the ultimate in engine protection. They provide an extra measure of protection for the investment in a spo.. |