Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 271 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 362 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 362CP-2 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 362CPT (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 363F (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 363F-UV (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 363F-WHITE (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 741E (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 706CS (IG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 706D-UV (IG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 902 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 902B (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | ASTM D97 |
Solvay Specialty Polymers FOMBLIN® M60 PFPE Lubricant Information provided by Solvay Solexis, Inc. |
|||
Pour Point | -60.0 °C | -76.0 °F | |
Teknor Apex TruVis Esters™ DIDA Di-IsoDecyl Adipate |
|||
Pour Point | -60.0 °C | -76.0 °F | ASTM D97 |
ExxonMobil 15 Mobil EAL Arctic Series Mobil EAL Arctic Series are high performance Environmental Awareness Lubricants (EAL) that are fully synthetic products designed specifically for the lubrication of refrigeration compressors and sys.. |
|||
Pour Point | -60.0 °C | -76.0 °F | |
ExxonMobil Mobil Avrex S Turbo 256 Mobil Avrex S Turbo 256 gas turbine lubricant is a combination of a highly stable synthetic base fluid and a unique chemical additive package. The combination provides outstanding thermal and oxid.. |
|||
Pour Point | -60.0 °C | -76.0 °F | ASTM D97 |
ExxonMobil Univis HVI 13 Exxon Univis HVI is a line of premium performance anti-wear hydraulic oils characterized by their unusually high viscosity indexes. They are engineered to maintain close viscosity control over wide .. |
|||
Pour Point | -60.0 °C | -76.0 °F | DIN ISO 3016 |
The Chemical Company VESTINOL® INB Benzoic Acid Isononyl Ester VESTINOL® INB is a new plasticizer based on benzoic acid and is not subject to any chemical classification and labeling requirements. The unique combination of low plastisol viscosity, combined wi.. |
|||
Pour Point | -60.0 °C | -76.0 °F | |
ExxonMobil Mobil Avrex M Turbo 201/1010 Mobil Avrex M Turbo 201/1010 gas turbine lubricant is a combination of a proven aviation engine mineral oil base stock and an ashless additive package. The effective operating range for Mobil Avrex .. |
|||
Pour Point | -60.0 °C | -76.0 °F | |
ExxonMobil Mobil Avrex S Turbo 256 Mobil Avrex S Turbo 256 gas turbine lubricant is a combination of a highly stable synthetic base fluid and a unique chemical additive package. The combination provides outstanding thermal and oxid.. |
|||
Pour Point | -60.0 °C | -76.0 °F | |
ExxonMobil Mobil Turbo 319A-2 Mobil Turbo 319A-2 is a fully synthetic lubricant developed to meet the performance requirements of Russian gas turbine aircraft engines which operate on mineral-oil-based lubricants. Formulated fro.. |
|||
Pour Point | -60.0 °C | -76.0 °F | ASTM D97 |
ExxonMobil Univis HVI 13 Exxon Univis HVI is a line of premium performance anti-wear hydraulic oils characterized by their unusually high viscosity indexes. They are engineered to maintain close viscosity control over wide .. |
|||
Pour Point | -60.0 °C | -76.0 °F | ASTM D97 |
ExxonMobil Univis HVI 26 Exxon Univis HVI is a line of premium performance anti-wear hydraulic oils characterized by their unusually high viscosity indexes. They are engineered to maintain close viscosity control over wide .. |
|||
Pour Point | -60.0 °C | -76.0 °F | ASTM D-97 |
ConocoPhillips ANDEROL® FGH 22 Synthetic Food Grade Hydraulic Fluid, ISO 22 Description: ANDEROL FGH Series Hydraulic Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA wh.. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 363 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 706D (IG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 783C (NG) Synthetic Oil Information provided by Nye Lubricants. |