Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -63.0 °C | -81.4 °F | Base Oil; ASTM D97 |
Nye Lubricants 825F-1 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -63.0 °C | -81.4 °F | Base Oil; ASTM D97 |
Nye Lubricants DHL-400 Oil Information provided by Nye Lubricants. |
|||
Pour Point | -63.0 °C | -81.4 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8311 (833-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -63.0 °C | -81.4 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8990 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -63.0 °C | -81.4 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8991MT (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -63.0 °C | -81.4 °F | |
PolyOne Synplast™ DOS-N Di (2-ethylhexyl) Sebacate Branched C8 sebacate esterInformation provided by PolyOne |
|||
Pour Point | -63.0 °C | -81.4 °F | Base Oil; ASTM D97 |
Nye Lubricants 833Z-1 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -63.0 °C | -81.4 °F | ASTM D97 |
Solvay Specialty Polymers FOMBLIN® Z60 PFPE Lubricant FOMBLIN® Z is a linear PFPE available as a neutral or functionalized fluid. They are used in aerospace, magnetic media, and polymer modification uses.Information provided by Solvay Solexis, Inc... |
|||
Pour Point | -63.0 °C | -81.4 °F | ASTM D97 |
ExxonMobil Mobil Synturion 6 Mobil Synturion 6 is a premium-quality, synthetic-base fluid specially formulated to meet the demanding lubrication and cooling requirements of mechanical seals --and to maximize seal life. The supe.. |
|||
Pour Point | -63.0 °C | -81.4 °F | ASTM D97 |
ChevronTexaco TEGRA® ISO 32 Synthetic Compressor Oil FeaturesChevron Tegra Synthetic Compressor Oils are synthetic compressor lubricants formulated with the highest quality polyalphaolefin (PAO) base fluids.They provide excellent thermal and oxidation.. |
|||
Pour Point | -63.0 °C | -81.4 °F | ASTM D97 |
ExxonMobil Mobil Synturion 6 Mobil Synturion 6 is a premium-quality, synthetic-base fluid specially formulated to meet the demanding lubrication and cooling requirements of mechanical seals --and to maximize seal life. The supe.. |
|||
Pour Point | -63.0 °C | -81.4 °F | ASTM D97 |
ChevronTexaco Aviation A Hydraulic Fluid FeaturesChevron Aviation Hydraulic Fluids are both manufactured from specially selected, highly refined, low viscosity and low pour point petroleum base stocks. They both contain a superior, shear .. |