Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -6.70 °C | 19.9 °F | |
ExxonMobil Thermrex Series F-43 The Thermrex Series is a family of four quench oils for the heat treatment of alloy steels. They are comprised of selected additives and solvent-refined base stocks to provide optimum chemical and .. |
|||
Pour Point | -6.70 °C | 19.9 °F | |
ExxonMobil Thermrex Series F-43 The Thermrex Series is a family of four quench oils for the heat treatment of alloy steels. They are comprised of selected additives and solvent-refined base stocks to provide optimum chemical and .. |