Polymer Property : Pour Point = 89.6 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Pour Point 32.0 °C
89.6 °F
ExxonMobil Kutwell 82
KUTWELL is the trademark for a line of two high-performance "soluble" cutting fluids for cooling and lubricating the tool and work in machining operations. The line includes one petroleum-base fluid..
Pour Point 32.0 °C
89.6 °F
ExxonMobil Kutwell 82
KUTWELL is the trademark for a line of two high-performance "soluble" cutting fluids for cooling and lubricating the tool and work in machining operations. The line includes one petroleum-base fluid..