Thermal Properties Metric English Comments
Strain Point 870 °C
1600 °F
Corning Vycor® 7907 UV-Blocking Glass
Vycor-UV™ is cerium-doped and provides homogeneous absorption of UV-B and UV-C.Special Features:Superior optical qualityTight dimensional controlThermal and chemical properties ideally suited to hi..