Polymer Property : Strain Point = 1967 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Strain Point 1075 °C
1967 °F
Varies with thermal history
Saint-Gobain HS Grade Optical Fused Quartz
HS Grade Optical Fused Quartz is a high purity, low [OH] natural fused quartz. It has excellent IR transmission, useful transmission from 260 to 3500 nm, excellent visual quality with low bubbles, ..