Thermal Properties Metric English Comments
Glow Wire Test 925 °C

@Thickness 2.00 mm
1700 °F

@Thickness 0.0787 in
GWIT; IEC 60695
Eurotec® Tecotek® PC40 GR10 NL PC, 10% glass fiber reinforced, natural
Information provided by Eurotec®
Glow Wire Test 925 °C

@Thickness 2.00 mm
1700 °F

@Thickness 0.0787 in
GWIT; IEC 60695
Eurotec® Tecotek® PC40 GR20 NL PC, 20% glass fiber reinforced, natural
Information provided by Eurotec®
Glow Wire Test 925 °C

@Thickness 2.00 mm
1700 °F

@Thickness 0.0787 in
GWIT; IEC 60695
Eurotec® Tecotek® PC40 GR30 NL PC, 30% glass fiber reinforced, natural
Information provided by Eurotec®