Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 969 °C @Thickness 3.00 mm |
1780 °F @Thickness 0.118 in |
0.8 mm wire; Ignition Temperature; IEC 60695-2-13 |
PolyOne Bergamid™ A700 G20 UF Polyamide 66 (Nylon 66) Information provided by PolyOne |