Polymer Property : UL RTI, Electrical = 167 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Electrical 75.0 °C

@Thickness 1.50 mm
167 °F

@Thickness 0.0591 in
UL 746
Polymer Resources PC/TP-GP2 PC/Polyester Alloy
High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b..
UL RTI, Electrical 75.0 °C

@Thickness 3.00 mm
167 °F

@Thickness 0.118 in
UL 746
Polymer Resources PC/TP-GP2 PC/Polyester Alloy
High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b..
UL RTI, Electrical 75.0 °C

@Thickness 0.749 mm
167 °F

@Thickness 0.0295 in
UL 746
Polymer Resources TP-FR-IM2 Polybutylene Terephthalate, Impact Modified, Flame Retardant, High Flow
Polybutylene Terephthalate, Impact Modified, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s..
UL RTI, Electrical 75.0 °C

@Thickness 1.50 mm
167 °F

@Thickness 0.0591 in
UL 746
Polymer Resources TP-FR-IM2 Polybutylene Terephthalate, Impact Modified, Flame Retardant, High Flow
Polybutylene Terephthalate, Impact Modified, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s..
UL RTI, Electrical 75.0 °C

@Thickness 3.00 mm
167 °F

@Thickness 0.118 in
UL 746
Polymer Resources TP-FR-IM2 Polybutylene Terephthalate, Impact Modified, Flame Retardant, High Flow
Polybutylene Terephthalate, Impact Modified, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s..
UL RTI, Electrical 75.0 °C

@Thickness 1.50 mm
167 °F

@Thickness 0.0591 in
UL 746
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced
Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov..
UL RTI, Electrical 75.0 °C

@Thickness 3.00 mm
167 °F

@Thickness 0.118 in
UL 746
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced
Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov..
UL RTI, Electrical 75.0 °C

@Thickness 1.50 mm
167 °F

@Thickness 0.0591 in
UL 746
Polymer Resources TP-IGFR-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced Warpage
Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmen..
UL RTI, Electrical 75.0 °C

@Thickness 3.00 mm
167 °F

@Thickness 0.118 in
UL 746
Polymer Resources TP-IGFR-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced Warpage
Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmen..
UL RTI, Electrical 75.0 °C

@Thickness >=2.10 mm
167 °F

@Thickness >=0.0827 in
LG Chemical AF312B ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
UL RTI, Electrical 75.0 °C

@Thickness >=2.50 mm
167 °F

@Thickness >=0.0984 in
LG Chemical AF312B ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
UL RTI, Electrical 75.0 °C

@Thickness >=3.00 mm
167 °F

@Thickness >=0.118 in
LG Chemical AF312B ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
UL RTI, Electrical 75.0 °C

@Thickness >=0.550 mm
167 °F

@Thickness >=0.0217 in
LG Chemical Lupox® GP1006FD PBT
Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica..
UL RTI, Electrical 75.0 °C

@Thickness >=0.800 mm
167 °F

@Thickness >=0.0315 in
LG Chemical Lupox® GP2400G PBT+GF40%
Description: Injection Molding, PBT+GF40%, HCFC ResistantApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 30965-26-5Information provided by LG Chemical
UL RTI, Electrical 75.0 °C

@Thickness >=3.00 mm
167 °F

@Thickness >=0.118 in
LG Chemical Lupox® GP2400G PBT+GF40%
Description: Injection Molding, PBT+GF40%, HCFC ResistantApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 30965-26-5Information provided by LG Chemical
UL RTI, Electrical 75.0 °C

@Thickness >=0.800 mm
167 °F

@Thickness >=0.0315 in
LG Chemical Lupox® NH2306F PBT+GF30%
Description: Injection Molding, PBT+GF30%, Halogen Free Flame RetardantApplication: IT/OA, E&E (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical
UL RTI, Electrical 75.0 °C

@Thickness >=1.60 mm
167 °F

@Thickness >=0.0630 in
LG Chemical Lupox® NH2306F PBT+GF30%
Description: Injection Molding, PBT+GF30%, Halogen Free Flame RetardantApplication: IT/OA, E&E (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical
UL RTI, Electrical 75.0 °C

@Thickness >=3.20 mm
167 °F

@Thickness >=0.126 in
LG Chemical Lupox® NH2306F PBT+GF30%
Description: Injection Molding, PBT+GF30%, Halogen Free Flame RetardantApplication: IT/OA, E&E (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical
UL RTI, Electrical 75.0 °C

@Thickness >=0.500 mm
167 °F

@Thickness >=0.0197 in
LG Chemical Lupox® TE5006F PET+PC
Description: Injection Molding, PET+PC, Flame Retardant, GWIT, CTIApplication: IT/OA, E&E (Connector)CAS No. 68928-70-1, 103598-77-2, 25038-59-9 and 1309-64-4Information provided by LG Chemical
UL RTI, Electrical 75.0 °C

@Thickness 0.930 mm
167 °F

@Thickness 0.0366 in
UL746B
DSM Arnite® A06 101 PET (European Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
UL RTI, Electrical 75.0 °C

@Thickness 3.00 mm
167 °F

@Thickness 0.118 in
UL746B
DSM Arnite® A06 101 PET (European Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
UL RTI, Electrical 75.0 °C

@Thickness 1.50 mm
167 °F

@Thickness 0.0591 in
UL746B
DSM Arnite® A04 900 PET (European Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
UL RTI, Electrical 75.0 °C

@Thickness 0.750 mm
167 °F

@Thickness 0.0295 in
UL746B
DSM Arnite® A04 900 PET (European Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
UL RTI, Electrical 75.0 °C

@Thickness 0.750 mm
167 °F

@Thickness 0.0295 in
UL746B
DSM Arnite® T06 204 SN PBT (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
UL RTI, Electrical 75.0 °C

@Thickness 3.00 mm
167 °F

@Thickness 0.118 in
UL746B
DSM Arnite® T06 204 SN PBT (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..