Polymer Property : UL RTI, Electrical = 239 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Electrical 115 °C

@Thickness 0.810 mm
239 °F

@Thickness 0.0319 in
UL 746
Teknor Apex Chemlon® 100 L Nylon 66, Unreinforced
Notes: Internally and externally lubricated; General Purpose; Double-lubricated for improved part ejection and machine feed Processing Method: Injection Molding Forms: PelletsInformation Provided by..
UL RTI, Electrical 115 °C

@Thickness 1.50 mm
239 °F

@Thickness 0.0590 in
UL 746
Teknor Apex Chemlon® 100 L Nylon 66, Unreinforced
Notes: Internally and externally lubricated; General Purpose; Double-lubricated for improved part ejection and machine feed Processing Method: Injection Molding Forms: PelletsInformation Provided by..
UL RTI, Electrical 115 °C

@Thickness 3.00 mm
239 °F

@Thickness 0.118 in
UL 746
Teknor Apex Chemlon® 100 L Nylon 66, Unreinforced
Notes: Internally and externally lubricated; General Purpose; Double-lubricated for improved part ejection and machine feed Processing Method: Injection Molding Forms: PelletsInformation Provided by..
UL RTI, Electrical 115 °C

@Thickness 0.810 mm
239 °F

@Thickness 0.0319 in
UL 746
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced
Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications. Processing Method: Injection Molding Forms: Pellets Automotive Specifications: ..
UL RTI, Electrical 115 °C

@Thickness 1.50 mm
239 °F

@Thickness 0.0590 in
UL 746
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced
Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications. Processing Method: Injection Molding Forms: Pellets Automotive Specifications: ..
UL RTI, Electrical 115 °C

@Thickness 3.00 mm
239 °F

@Thickness 0.118 in
UL 746
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced
Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications. Processing Method: Injection Molding Forms: Pellets Automotive Specifications: ..