Thermal Properties Metric English Comments
UL RTI, Mechanical with Impact 160 °C

@Time 2.16e+7 sec
320 °F

@Time 6000 hour
Solvay TECHNYL® A 60 G1 V30 PA66, 30% glass fiber, DRY