Working Point 960 °C
1760 °F
Viscosity 10<sup>4</sup> dPa s; ISO 7884-2
Schott Glass 8100 Lead Glass
Lead glass (33.5% PbO), electrically highly insulating, highly x-ray-absorbing TV tubesInformation provided by SCHOTT AG.