Polymer Property : Distillation Temperature = 165 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Distillation Temperature <= 165 °C
<= 329 °F
0.5
Unipetrol C9 Fraction Redistillated
C9 fraction redistillated (RC9) is a distillation cut of pyrolysis gasoline, produced as a by-product during manufacture of ethylene. It is a transparent, colourless to yellowish liquid with prevail..