Brittleness Temperature -2.00 °C
28.4 °F
ASTM D746-79
DuPont Performance Polymers Hypalon® 48 Chlorosulfonated Polyethylene Rubber, Uncured Carbon Black Filled Compound &
Carbon black compound with 100 parts Hypalon; 100 parts carbon black; 4 parts magnesia; and 1.5 parts propylene glycol. Physical property data below (except mooney viscosity) are for uncured film. ..
Brittleness Temperature -2.00 °C
28.4 °F
ASTM D746
Teknor Apex APEX® 60001-L Polyvinyl Chloride, Flexible
Notes: RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex
Brittleness Temperature -2.00 °C
28.4 °F
ASTM D746
Colorite Polymers CS7559LS Wire and Cable Insulation Vinyl Compound
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai..