Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable WEMB410 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable WEMB410U Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible B5DW2 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R8180K Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible XV3785 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D746A |
Solvay Specialty Polymers Solef® 21508 PVDF Copolymer
(discontinued **) Key features of this grade: High Elongation, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® P.. |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D746 |
Teknor Apex APEX® 2595-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D746 |
Teknor Apex APEX® 3200-85 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D746 |
Teknor Apex APEX® 3311-90 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D746 |
Teknor Apex APEX® 3601-95 Polyvinyl Chloride, Flexible Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: Second Generation SeriesInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D746 |
Teknor Apex APEX® 84455 Polyvinyl Chloride, Flexible Notes: 105°C Insulation; RoHS Compliant Features: Flame RetardantUses: Insulation Agency Ratings: UL 1063; UL 62; UL 1581 Forms: Pellets Wire Types: AWMInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D746 |
Teknor Apex APEX® 80128-Y Polyvinyl Chloride, Flexible Notes: 75°C Insulation; RoHS CompliantFeatures: Sunlight Resistant (720 hours) Uses: Cable Jacketing; InsulationAgency Ratings: UL QMTT2 .E73402; UL 1063; UL 1581; UL 62; UL 83Forms: Pellets Wire.. |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | |
Daikin DAI-EL G-783 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Fast vulcanization, for complex shapes.Information provided by Daikin .. |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds CL 86/6 Flexible PVC, Sheathing General purposes |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 8502 Flexible PVC, Injection Molding for Footwear Soles |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D746 |
Colorite Polymers CS1521SC Non Lead Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D746 |
Colorite Polymers CS1524SP Non Lead Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D746 |
Colorite Polymers CS9034SR Wire and Cable Insulation Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D746 |
Colorite Polymers 7342 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PH 70/AS Flexible PVC, Transparent Extrusion Food belt carriers |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PH 75/C Flexible PVC, Transparent Extrusion Profiles, UL 94 Class V1 |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D-746 |
Axiall 8820 Moldings & Extrusions Flexible PVC General purpose extrusion and molding compound designed for use in weatherstrips, screen spline and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 201.. |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D746 |
Alliance Polymers Zythane™ 4045D Thermoplastic Polyurethane Elastomer Zythane™ 4045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D-746 |
Axiall 16930 Wire & Cable Flexible PVC Non-lead stabilized tray cable jacketing compound. UL recognized component for 720 hour sunlight resistance in black only.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation .. |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D-746 |
Axiall 17940 Wire & Cable Flexible PVC THW insulation compound. Also suitable for 105C applications in 3/64 and larger sizes. UL recognized component for THW. Oil resistant I, VW-1 rated.Information provided by Georgia GulfGeorgia Gul.. |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | |
AlphaGary GW 2038 VW1 LCF Flame Retardant Polyvinyl Chloride 60°C or 75°C rated jacketing compound for CMR cable per UL 444 |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D746 |
Teknor Apex APEX® 3210-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D746A |
Solvay Specialty Polymers Solef® 20810 PVDF Copolymer
(discontinued **) Key features of this grade: Li Battery, Virgin. Recommended processing is solution. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | ASTM D-746 |
Axiall 34431 Wire & Cable Flexible PVC TW insulation. UL recognized for TW, Oil resistant I and VW-1.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -22.0 °C | -7.60 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 8004 Flexible PVC, Injection Molding for Footwear Soles |