Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -31.1 °C | -24.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible C8500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -31.1 °C | -24.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible SL9994 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -31.1 °C | -24.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible H43356A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -31.1 °C | -24.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R158AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |