Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -28.9 °C | -20.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable WJAC38 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -28.9 °C | -20.0 °F | ASTM D746 |
PolyOne Geon™ HC 2175 Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2175 is a 75 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2175 can be used for extrusion and injection molding healthcare applications.NOTE: All ing.. |
|||
Brittleness Temperature | -28.9 °C | -20.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R100AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -28.9 °C | -20.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R275AE White 685 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -28.9 °C | -20.0 °F | ASTM D746 |
PolyOne Geon™ HC 2175G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2175G is a 75 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2175G can be used for extrusion and injection molding healthcare applicatio.. |
|||
Brittleness Temperature | -28.9 °C | -20.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R1212A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |