Brittleness Temperature -59.4 °C
-75.0 °F
ASTM D746-95
Saint-Gobain Norprene® A-60-F Food Process Tubing Formulation
Description: Norprene® Food Process Tubing, Formulation A-60-F: Formulated to withstand the high temperatures frequently occurring during food and beverage processing, Norprene® Food Process..
Brittleness Temperature -59.4 °C
-75.0 °F
ASTM D746-98
Saint-Gobain Norprene® A-60-G Industrial Grade Tubing Formulation
Description: Norprene® Industrial Grade Tubing, Formulation A-60-G: Norprene® Industrial Grade Tubing outperforms neoprene, EPDM and other general-purpose tubings in test after test and appl..
Brittleness Temperature -59.4 °C
-75.0 °F
ASTM D746
Saint-Gobain Tygon® Noroprene® Chemical Tubing Formulation
Norprene® Chemical Tubing is a high performance co-extruded product specifically formulated to provide an ideal combination of chemical resistance and pump life. Its inert ultra-smooth plasticize..
Brittleness Temperature -59.4 °C
-75.0 °F
ASTM D746-98
Saint-Gobain Tygon® Norprene® A-60-F I.B. Pressure Tubing Formulation for CIP and SIP cleaning and sterilization systems
Good for use in clean-in-place and steam-in-place cleaning and sterilization systems, Norprene® Pressure Tubing has excellent alkali resistance and is compatible with numerous oxidizing agents su..
Brittleness Temperature -59.4 °C
-75.0 °F
ASTM D746-98
Saint-Gobain Tygon® Norprene® A-60-N Drinking Water Tubing Formulation.
Formulated for use as drinking water tubing. Complies with FDA and NSF61 criteria.Information provided by Saint Gobain Performance Products.
Brittleness Temperature -59.4 °C
-75.0 °F
ASTM D746; ISO 812
Advanced Polymer Alloys Alcryn® 4680 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..