Brittleness Temperature -52.2 °C
-62.0 °F
ASTM D746
PolyOne Geon™ Vinyl Wire & Cable JA612EA Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -52.2 °C
-62.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible R5145B Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -52.2 °C
-62.0 °F
ASTM D746
ExxonMobil Santoprene® 121-65M300 Thermoplastic Elastomer  (discontinued **)
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and good..
Brittleness Temperature -52.2 °C
-62.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible R5145A Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -52.2 °C
-62.0 °F
ASTM D746
ExxonMobil Santoprene® 103-40 Thermoplastic Elastomer
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..