Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Brittleness Temperature = -7.06 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -21.7 °C
-7.06 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible D75M0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -21.7 °C
-7.06 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible B80MB Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne