Brittleness Temperature -7.22 °C
19.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible F70E Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -7.22 °C
19.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible F77E Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne