Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -66.7 °C | -88.0 °F | ASTM D 746 |
CPT C-Flex® R70-082 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |