Polymer Property : Brittleness Temperature = 1.40 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -17.0 °C
1.40 °F
ASTM D746
PolyOne Geon™ Vinyl Wire & Cable W1820L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Brittleness Temperature -17.0 °C
1.40 °F
ASTM D746
S&E Specialty Polymers GA-3133S-CCUV PVC
Application: Meets style 1277 T.C. Power & Control Cable Requirements and can be used for CM(X), CATV(X) and CL2 jacketing applications. UL listed for 720hr. sunlightInformation provided by S&E Spec..
Brittleness Temperature -17.0 °C
1.40 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible R1480E Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Brittleness Temperature -17.0 °C
1.40 °F
ASTM D746
LyondellBasell Montell 8340 Polybutene-1
Key Features: semi-crystalline low ethylene content random copolymer, miscible with polypropylenes, FDA acceptableApplications: minor additive in a polyethylene peel seal layerMeets FDA requirements..
Brittleness Temperature -17.0 °C
1.40 °F
ASTM D746
Teknor Apex APEX® 153 Polyvinyl Chloride Compound
Notes: Non-Migrating; Sunlight Resistant Jacket Temperature Rating: 105°CInformation Provided by Teknor Apex
Brittleness Temperature -17.0 °C
1.40 °F
ASTM D746
Teknor Apex APEX® 460 Polyvinyl Chloride, Flexible
Notes: 105°C Insulation; RoHS Compliant Features: Low to no Migration; Oil Resistant Uses: Flexible Cord InsulationForms: Pellets Wire Types: SJTOO; STOO Processing Method: Extrusion Additional I..
Brittleness Temperature -17.0 °C
1.40 °F
ASTM D746
Teknor Apex APEX® 590 Polyvinyl Chloride, Flexible
Notes: RoHS Compliant Features: General Purpose Uses: Tubing; Wire Jacketing Agency Ratings: UL 498; UL 62 Wire Types: SPT-1; SPT-2 Processing Method: Injection MoldingForms: PelletsInformation Prov..
Brittleness Temperature -17.0 °C
1.40 °F
ASTM D746
Teknor Apex APEX® 65005 Polyvinyl Chloride, Flexible
Notes: 75°C Jacket; RoHS Compliant Features: Flame Retardant Uses: Communication Wire Jacketing Forms: Pellets Agency Ratings: NEC Article 725; NEC Article 760; NEC Article 770; NEC Article 800; ..
Brittleness Temperature -17.0 °C
1.40 °F
ASTM D746
Teknor Apex APEX® 7500-105 Polyvinyl Chloride, Flexible
Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL..
Brittleness Temperature -17.0 °C
1.40 °F
ASTM D746
Teknor Apex MF 165 D NT Polyvinyl Chloride, Flexible Film
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsInformation provided by Teknor Apex Company
Brittleness Temperature -17.0 °C
1.40 °F
ASTM D746
Teknor Apex MF 165 NT Polyvinyl Chloride, Flexible Film
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsAppearance-ClearInformation provided by Teknor Apex Company
Brittleness Temperature -17.0 °C
1.40 °F
Sylvin Technologies 504 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Brittleness Temperature -17.0 °C
1.40 °F
ASTM D746
Teknor Apex APEX® 84853-L Polyvinyl Chloride, Flexible
Notes: 105°C Insulation; RoHS CompliantFeatures: Flame Retardant; High Heat Resistant Uses: InsulationAgency Ratings: UL 62 Forms: Pellets Wire Types: SJT; ST; SVTInformation Provided by Teknor A..
Brittleness Temperature -17.0 °C
1.40 °F
Daikin DAI-EL G-701 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content
Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: General purpose with excellent compression set.Information provided by..
Brittleness Temperature -17.0 °C
1.40 °F
Daikin DAI-EL G-751 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content
Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: General purpose with excellent metal bonding and compression set.Infor..
Brittleness Temperature -17.0 °C
1.40 °F
ASTM D746
Colorite Polymers CS1533UL Wire and Cable Jacket Vinyl Compound
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai..
Brittleness Temperature -17.0 °C
1.40 °F
ASTM D-746
Axiall H 5177B Plenum Flexible PVC
Plenum-grade jacket with good low temperature properties for use over 100% FEP primaries. UL QMTM2 plenum cable compound component.Information provided by Georgia GulfGeorgia Gulf became Axiall Cor..
Brittleness Temperature -17.0 °C
1.40 °F
ASTM D-746
Axiall 2258 Wire & Cable Flexible PVC
TW insulation suitable for 105°C AWM applications. UL recognized for TW, Oil resistant I and VW-1.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Brittleness Temperature -17.0 °C
1.40 °F
ASTM D746
Teknor Apex APEX® 3202-85 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Caps, Closure, Connectors, Food Service Applications, Safety Equipment, Valves/Valve Parts Appearance-Cl..
Brittleness Temperature -17.0 °C
1.40 °F
ASTM D746A
Solvay Specialty Polymers Solef® 11008 PVDF Copolymer  (discontinued **)
Key features of this grade: Low Viscosity, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVD..
Brittleness Temperature -17.0 °C
1.40 °F
ASTM D-746
Axiall 46801 Coax & Telecom Flexible PVC
Semi-rigid flame retardant compound suitable for telecom insulation applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.