Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -7.00 °C | 19.4 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W1349L-xx09FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Brittleness Temperature | -7.00 °C | 19.4 °F | ASTM D746 |
Teknor Apex APEX® 3210-90 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Brittleness Temperature | -7.00 °C | 19.4 °F | TR-10 |
DuPont Performance Polymers VTR 8710 (ETP-600S) Peroxide Cured Fluoroelastomer (FKM) Formulation
(discontinue FormulationViton® Extreme™ ETP-600S |