Brittleness Temperature -1.00 °C
30.2 °F
AlphaGary Smokeguard™ LS III 1096 Low Smoke Polyvinyl Chloride
60°C Plenum Jacket
Brittleness Temperature -1.00 °C
30.2 °F
Plasticizer conc. in vinyl film 33 phr; ASTM D746
BASF Palamoll® 656 Polymeric Plasticizer
Description: Palamoll® 656 is a high viscosity polymeric plasticizer that is compatible with PVC. It is based on adipic acid and polyhydric alcohols. It is resistant to oils, fats, aliphatic hydro..