Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | 8.00 °C | 46.4 °F | |
Colorite Polymers 9811 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
Brittleness Temperature | 8.00 °C | 46.4 °F | |
Colorite Polymers 9812 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |