Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 40.0 °C
104 °F
ISO 75-1/-2
Lanxess Durethan® B 31 F 000000 Nylon 6, Film Grade
PA 6, film grade, low viscosity, easy flow, additive-freeApplication Examples: flat and blown film, monofilaments, coatings
Deflection Temperature at 8.0 MPa 40.0 °C
104 °F
Lanxess Durethan® B 35 F 000000 Nylon 6, Extrusion, Low Viscosity
PA 6, non-reinforced, extrusion, low viscosity, no additivesInformation provided by LANXESS.
Deflection Temperature at 8.0 MPa 40.0 °C
104 °F
ISO 75-1/-2
Lanxess Durethan® B 35 FA 000000 Nylon 6, Film Grade
PA 6, film , medium viscosity, lubricated, not nucleated, in compliance with FDA for food contact and acc. the German BgVV Recommendation XLIV, Section VI.A" Synthetic casings in polyamide"Applicati..
Deflection Temperature at 8.0 MPa 40.0 °C
104 °F
ISO 75-1/-2
Lanxess Durethan® B 35 FKA 000000 Nylon 6, Film Grade
PA 6 Film grade, medium viscosity, nucleated, with processing and slip additives, in compliance with FDA for food contactApplication Examples: flat and blown film, flat film coextrusion for PA/PE co..
Deflection Temperature at 8.0 MPa 40.0 °C
104 °F
ISO 75-1/-2
Lanxess Durethan® B 38 FKA 000000 Nylon 6, Film Grade
PA 6 film-grade, medium to higher viscosity, with processing aid and slip agent, nucleated, in compliance with FDA for food contactApplication Examples: flat and blown film, flat film coextrusion fo..
Deflection Temperature at 8.0 MPa 40.0 °C
104 °F
ISO 75-1/-2
Lanxess Durethan® B 40 E 000000 Nylon 6
PA 6 extrusion grade, standard grade of high viscosity with processing aid/lubricant, not nucleated.
Deflection Temperature at 8.0 MPa 40.0 °C
104 °F
ISO 75-1/-2
Lanxess Durethan® B 40 F 000000 Nylon 6, Film Grade
PA 6, Film grade, high viscosity, without additives or processing aids, in compliance with FDA for food contact and acc. the German BgVV Recommendation XLIV, Section VI.A" Synthetic casings in polya..
Deflection Temperature at 8.0 MPa 40.0 °C
104 °F
ISO 75-1/-2
Lanxess Durethan® B 40 FA 000000 Nylon 6, Film Grade
PA 6, film grade of high viscosity, lubricated, not nucleated, in compliance with FDA for food contact and acc. the German BgVV Recommendation XLIV, Section VI.A" Synthetic casings in polyamide"Appl..
Deflection Temperature at 8.0 MPa 40.0 °C
104 °F
ISO 75-1/-2
Lanxess Durethan® B 40 FAM 000000 Nylon 6, Film Grade
PA 6 film grade of high viscosity with high slip agent and lubricant content, not nucleatedApplication Examples: flat and blown film with good surface slip and smoothness - including in the freshly ..
Deflection Temperature at 8.0 MPa 40.0 °C
104 °F
ISO 75-1/-2
Lanxess Durethan® B 40 FKA 000000 Nylon 6, Film Grade
PA 6 film grade of high viscosity, nucleated and lubricated, in compliance with FDA for food contactApplication Examples: flat and blown film, flat film coextrusion for PA/PE composite films
Deflection Temperature at 8.0 MPa 40.0 °C
104 °F
ISO 75-1/-2
Lanxess Durethan® BC 304 H3.0 000000 Nylon 6
PA 6, injection molding grade, non-reinforced, elastomer-modified, extremely high notched impact strength, including in the dry state and at low temperatures, also applicable for barrier layers in e..
Deflection Temperature at 8.0 MPa 40.0 °C
104 °F
ISO 75-1/-2
EMS-Grivory Grivory® LKN-5H PA12-GB50
Product description: Grilamid LKN-5H is a 50% glass bead reinforced, heat stabilized polyamide 12 injection molding grade with the following property profile: Very low moisture absorptionExtremely g..
Deflection Temperature at 8.0 MPa 40.0 °C
104 °F
ISO 75-1/-2
EMS-Grivory Grivory® LKN-3H PA12-GB30