Polymer Property : Deflection Temperature at 8.0 MPa = 139 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 139 °C
282 °F
Unannealed; ISO 75-2/C
PolyOne OnForce™ LFT PP-40LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Deflection Temperature at 8.0 MPa 139 °C
282 °F
Unannealed; ISO 75-2/C
PolyOne OnForce™ LFT PP-50LGF/001 UV Black Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..