Polymer Property : Deflection Temperature at 8.0 MPa = 168 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 168 °C
334 °F
ISO 75 Cf
Vyncolit BXE7665 Glass Filled Phenolic Molding Compound
Novolac resin based, mainly glass fiber filled. Excellent electrical properties combined with very good mechanical properties. Grade especially suitable for electrical applications.Information pro..