Polymer Property : Deflection Temperature at 8.0 MPa = 171 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 171 °C
340 °F
ISO 75 Cf
Vyncolit BXE7670 Glass Filled Phenolic Molding Compound
Novolac resin based, mainly glass fiber filled. Due to its unique composition, excellent balance between mechanical, thermal and dimensional stability.Information provided by Sumitomo Bak North Ame..