Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 8.0 MPa | 185 °C | 365 °F | ISO 75-2 |
Hexion Bakelite™ PF 4109 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, low shrinkage, high mechanical strength, U.. |
|||
Deflection Temperature at 8.0 MPa | 185 °C | 365 °F | ISO 75-1,-2 |
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers PA 66, 30% glass fibers, injection molding, heat-ageing stabilized |
|||
Deflection Temperature at 8.0 MPa | 185 °C | 365 °F | ISO 75-1/-2 |
Lanxess Durethan® AKV 35 H2.0 901510 Nylon 66, 35% Glass Fiber PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistanceApplication Examples: gearbox oil sumps, oil modules |
|||
Deflection Temperature at 8.0 MPa | 185 °C | 365 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GVS-5H nat PA*-GF50 Product description: Grivory GVS-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide.. |
|||
Deflection Temperature at 8.0 MPa | 185 °C | 365 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSC-20/4 EC black 9832 PA666-CF20 Information provided by EMS Grivory |
|||
Deflection Temperature at 8.0 MPa | 185 °C | 365 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSC-30/4 EC black 9832 PA666-CF30 Product description: Grilon TSC-30/4 EC is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% carbon fibers. Grilon TSC-30/4 EC has the following important properties:El.. |
|||
Deflection Temperature at 8.0 MPa | 185 °C | 365 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSC-40/4 EC black 9832 PA666-CF40 Information provided by EMS Grivory |
|||
Deflection Temperature at 8.0 MPa | 185 °C | 365 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GVS-5H black 9915 PA*-GF50 Product description: Grivory GVS-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Deflection Temperature at 8.0 MPa | 185 °C | 365 °F | HDT/C; ISO 75-2 |
Akro-Plastic Akromid® B3 GF 50 (2475) PA 6 Dry, 50% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Deflection Temperature at 8.0 MPa | 185 °C | 365 °F | ISO 75-2 |
Hexion Bakelite™ PF 4111 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free, Copper Adhesive Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, high mechanical strength, copper-adhesive,.. |