Polymer Property : Deflection Temperature at 8.0 MPa = 85.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 85.0 °C
185 °F
ISO 75-1/-2
EMS-Grivory Grivory® BGZ-30/2 PA6-GF30
Product description: Grilon BGZ-30/2 is a heat stabilized and impact modified PA6 injection molding grade with 30% glass fibers. Grilon BGZ-30/2 has the following important properties: Good impact s..
Deflection Temperature at 8.0 MPa 85.0 °C
185 °F
ISO 75-1/-2
EMS-Grivory Grivory® HT3Z LF black 9564 PA*
Product description: Grivory HT3Z LF is an unreinforced and impact resistant, PTFE modified engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT produc..
Deflection Temperature at 8.0 MPa 85.0 °C
185 °F
ISO 75-1/-2
EMS-Grivory Grivory® TSGZ-25/4 PA666-GF25
Information provided by EMS Grivory
Deflection Temperature at 8.0 MPa 85.0 °C
185 °F
ISO 75-1/-2
EMS-Grivory Grivory® BGZ-30 PA6-GF30
Product description: Grilon BGZ-30 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 30% glass fibers. Grilon BGZ-30 has the following important properties:..
Deflection Temperature at 8.0 MPa 85.0 °C
185 °F
ISO 75-1/-2
Lanxess Pocan® A 3131 000000 PBT+ASA, 30% glass fibers
PBT+ASA, 30% glass fibers, injection molding, low tendency to warp, improved surface finish