Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 47.10 °C
116.8 °F
ASTM D648
CRP Technology Windform® FX Polyamide Composite
Processed by selective laser sintering (SLS). Windform® FX is a new generation polyamide based material, whose repeatability and mechanical characteristics make it particularly suited for Additive..