Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 43.3 - 54.4 °C | 110 - 130 °F | ASTM D648 |
Arkema Group Kynar Flex® 3120 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 48.9 - 54.4 °C | 120 - 130 °F | Average value: 51.1 °C Grade Count:5 |
Overview of materials for Nylon 11 with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with PTFE Filler". Each property range of values reported is minimum and maximum values of appr.. |