Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 91.7 °C | 197 °F | Unannealed; ASTM D648 |
M. Holland Company GS411 Polystyrene
(discontinued **) Features: Good Crack Resistance, Crystal, Fast Cycle (Production), Good FlowUses: Disposable Drinkware, Electrical/Electronic ApplicationsApprovals: FDA 21 CFR 177.1640 Processing Method: Extrusio.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.7 °C | 197 °F | ASTM D648 |
Quantum Nylon 6/6 Information provided by Quantum Advanced Engineering Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.7 °C | 197 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hybrid B2035I Polycarbonate + PBT Alloy Available in North America High Impact Resistance Form: PelletsInformation provided by Ravago |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 91.7 °C | 197 °F | Unannealed; ASTM D648 |
M. Holland Company IS200 Polystyrene, High Impact
(discontinued **) Uses: Audio Tapes, Household Goods, ToysProcessing Method: Injection MoldingInformation provided by M. Holland. |