Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 127 - 235 °C
261 - 455 °F
Average value: 178 °C Grade Count:5
Overview of materials for Nylon 66/6, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl..
Deflection Temperature at 1.8 MPa (264 psi) 125 - 235 °C
257 - 455 °F
Average value: 150 °C Grade Count:23
Overview of materials for Polyphenylene Ether, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu..