Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 289 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 289 °C
552 °F
Unannealed; ISO 75-2/A
PolyOne OnForce™ LFT AM-40LGF/001 Natural Polyphthalamide (PPA)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Deflection Temperature at 1.8 MPa (264 psi) 289 °C
552 °F
Unannealed; ASTM D648
LNP Thermocomp® STN-F-1006 HS Polyamide 46, Glass Fiber Reinforcement  (discontinued **)
Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti..
Deflection Temperature at 1.8 MPa (264 psi) 289 °C

@Thickness 3.20 mm
552 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP UX04509 PPA
LNP* Thermocomp* UX04509 is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Deflection Temperature at 1.8 MPa (264 psi) 289 °C
552 °F
ASTM D648
E-Polymers SEPAZ® C230GI 30% Glass Fiber Reinforced Good Impact LCP Resin
Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding ..