Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 294 °C | 561 °F | Unannealed; ISO 75-2/A |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 294 °C | 561 °F | ASTM D648 |
Solvay Specialty Polymers Amodel® AF-4133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced
(discontinued AMODEL AF-4133 V0 is a 33% glass reinforced grade of polyphthalamide (PPA) resin that was designed specifically to process with water-cooled molds and meet the requirements of most electrical/electr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 294 °C | 561 °F | Unannealed; ISO 75-2/A |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 294 °C | 561 °F | Unannealed; ISO 75-2/A |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp.. |