Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 296 °C
565 °F
Unannealed; ISO 75-2/Af
Solvay Specialty Polymers Amodel® A-1133 DW Polyphthalamide (PPA)  (discontinued **)
Amodel A-1133 DW is a 33% glass-fiber reinforced polyphthalamide (PPA) grade approved for use with potable water in the United States, the United Kingdom and France. - Natural: A-1133 NT DW - Black:..
Deflection Temperature at 1.8 MPa (264 psi) 296 °C
565 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP Lubricomp LFL36 PEEK
LNP* Lubricomp* LFL36 is a compound based on PEEK containing Glass Fiber and PTFE.This data was supplied by SABIC-IP for the Americas region.
Deflection Temperature at 1.8 MPa (264 psi) 296 °C
565 °F
Unannealed; Flatwise; ISO 75-2/A
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA), 33% Glass Fiber
Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; ..
Deflection Temperature at 1.8 MPa (264 psi) 296 °C
565 °F
Unannealed; ISO 75-2/Af
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA)  (Unverified Data**)
Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade. Natural: HFZ A-1133 L NT Black: HFZ A-1133 L BK 937Information provided by Solvay Specialty Polymers.