Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 148 °C
299 °F
Unannealed; ASTM D648
Ravago Manufacturing Americas Echo® RPC30G BK Polypropylene Homopolymer
Available in North America Filler: Glass Fiber Reinforcement, 30% Filler by weight Recycled Content: YesFeatures: Homopolymer Color: Black Form: Pellets Information provided by Ravago