Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 301 °C
574 °F
ASTM D648
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded  (d
AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, ..
Deflection Temperature at 1.8 MPa (264 psi) 301 °C
574 °F
Unannealed; ASTM D648
Techmer ES HiFill® PPA GF30 HS L 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthInformat..
Deflection Temperature at 1.8 MPa (264 psi) 301 °C
574 °F
Unannealed; ASTM D648
Techmer ES HiFill® TPX-HTN-01027 A 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthUL File ..
Deflection Temperature at 1.8 MPa (264 psi) 301 °C
574 °F
Unannealed; ASTM D648
Techmer ES Luriblend® HTN 01400 BK
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, High Heat Resistance and LubricatedAppearance: BlackInformation provided by TP Composites, ..