Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 154 - 177 °C | 310 - 351 °F | Average value: 166 °C Grade Count:13 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | ASTM D648 |
Fiberfil® J-69/30/E/M High performance polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | ASTM D648 |
Fiberfil® J-69/20/E High performance polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | ASTM D648 |
Fiberfil® J-69/40/E High performance polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® POM CO GF15 CC 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 15% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP E GF40 CC 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Chemically Coupled, Heat Stabilized and High Viscosit.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF20 CC HF 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High FlowInformation provided by .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF20 CC LE 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Chemically Coupled and Low ExtractablesInformation provided by TP Composites, .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF50 CC HF BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® POM CO CF10 TL10 BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE Lubricant(10%)Features: Lubricated and CopolymerUL File: E157318Information provided b.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | ASTM D648 |
Asahi Kasei Thermylene® P7-30FG-0790 30% Glass Fiber Reinforced, Impact Modified Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | ASTM D648 |
Asahi Kasei Thermylene® P7-30FG-0874 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | ASTM D648 |
Asahi Kasei Thermylene® P7-30FG-1804 30% Glass Fiber Reinforced, Chemically Coupled Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | ASTM D648 |
Asahi Kasei Thermylene® P7-40FG-0790 40% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | ASTM D648 |
Asahi Kasei Thermylene® P7-40FG-0874 40% Glass Fiber Reinforced, Impact Modified Information provided by Asahi Thermofil |