Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 157.22 °C
315.00 °F
ASTM D648
Lucent Polymers GPB-115 Polybutylene Terephthalate, 15% Glass Fiber Reinforced
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 157.22 °C
315.00 °F
ASTM D648
Lucent Polymers GPB-130 Polybutylene Terephthalate, 30% Glass Fiber Reinforced
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 157.22 °C
315.00 °F
ASTM D648
Lucent Polymers GPB-FR515 Polybutylene Terephthalate, 15% Glass Fiber Reinforced, Flame Resistant
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.