Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 350 °C | 662 °F | DIN 53 461 |
Ensinger TECASINT™ 2022 Polyimide, Black, 15% Graphite (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 350 °C | 662 °F | |
LATI Latilub 88/10-15T K/30 PEEK, 30% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyetheretherketone (PEEK). PTFE. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |