Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 37.3 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 37.3 °C
99.1 °F
ASTM D648
NOVA Chemicals Novapol® TR-0735-U Hexene MDPE Rotational Molding Resin
Good impact resistance, Excellent processabilityApplications: Toys, Complex custom parts, Home and garden items, MailboxesAdditives: Processing antioxidants, UV stabilizersInformation provided by NO..
Deflection Temperature at 1.8 MPa (264 psi) 37.3 °C
99.1 °F
ASTM D648
NOVA Chemicals Novapol® TR-0735-UG Hexene MDPE Rotational Molding Resin
Features: Good impact properties Excellent processabilityNSF listed for Stds. 14, 24 and 61 Applications: ToysComplex custom partsHome and garden itemsMailboxesInformation provided by Nova Chemicals..
Deflection Temperature at 1.8 MPa (264 psi) 37.3 °C
99.1 °F
ASTM D648
NOVA Chemicals Novapol® PR-0636-UG Butene MDPE Rotational Molding Resin  (discontinued **)
Very good processability, Very good ESCR, Good impact properties, NSF listed for Stds. 14, 24, and 61Applications: Toys, General purpose custom molding, Carts, Playground equipmentAdditives: Process..
Deflection Temperature at 1.8 MPa (264 psi) 37.3 °C
99.1 °F
ASTM D648
NOVA Chemicals Sclair® TD-7915-UG Hexene MDPE Rotational Molding Resin  (discontinued **)
Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera..
Deflection Temperature at 1.8 MPa (264 psi) 37.3 - 41.0 °C
99.1 - 106 °F
Average value: 38.4 °C Grade Count:12
Overview of materials for Medium Density Polyethylene (MDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim..
Deflection Temperature at 1.8 MPa (264 psi) 37.3 °C
99.1 °F
ASTM D648
NOVA Chemicals Sclair® TD-7915-U Hexene MDPE Rotational Molding Resin  (discontinued **)
Excellent low temperature impact properties, Excellent ESCR, Wide process window, NSF listing for Stds. 14, 24, and 61 pending, Retention of impact at long cook timesApplications: IBCs, Toys, Genera..
Deflection Temperature at 1.8 MPa (264 psi) 37.3 - 42.0 °C
99.1 - 108 °F
Average value: 40.4 °C Grade Count:3
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu..
Deflection Temperature at 1.8 MPa (264 psi) 37.3 °C
99.1 °F
ASTM D648
NOVA Chemicals Novapol® PR-0636-U Butene MDPE Rotational Molding Resin  (discontinued **)
Very good processability, Very good ESCR, Good impact properties, NSF listed for Stds. 14, 24, and 61Applications: Toys, General purpose custom molding, Carts, Playground equipmentAdditives: Process..