Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 410 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 410 °C
770 °F
ASTM D-648
PlastiComp Complet® LCF30-PES Polyethersulfone, 30% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyethersulfone with 30% long carbon fiber reinforcementInformation provided by Plast..