Deflection Temperature at 1.8 MPa (264 psi) 212.8 °C

@Thickness 6.40 mm
415.0 °F

@Thickness 0.252 in
Unannealed; ASTM D648
LG Chemical LUMID SG2600B PA6+GF60%, General purpose, Good Surface
Feature: Injection Molding, PA6+GF60%, General purpose, Good SurfaceApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical